An efficient and economic approach is proposed for the fast and direct recovery of silica materials from photonic waste powder. Unlike the conventional alkaline fusion method for the extraction of silica from waste materials, this method possesses advantages of a rapid and low-energy-consumed process with total recovery yield. The obtained mesoporous silica material, denoted as MCM-41(DU)-F, was recovered directly from photonic waste powder at room temperature with the assistance of cationic surfactant, hydrofluoric acid, and ammonia hydroxide. The recycled MCM-41(DU)-F with a high specific surface area (788 m2/g), ordered mesoporous structure (4.5 nm), and large pore volume (1.1 cm3/g) was used as support of tetraethylenepentamine (TEPA) for the capture of CO2 from a flue gas stream. The results demonstrated that TEPA-impregnated MCM-41(DU)-F had an adsorption capacity of 120 mg of CO2/g of adsorbent. This is higher than the amount adsorbed by TEPA-MCM-41(NaSi) made from pure chemicals (113 mg of CO2/g o...

Autoren:   Liang-Yi Lin; Hsunling Bai
Journal:   Environmental Science & Technology
Jahrgang:   2013
DOI:   10.1021/es301504w
Erscheinungsdatum:   05.04.2013

Merkliste

Hier setzen Sie die nebenstehende Fachpublikation auf Ihre persönliche Merkliste.

Zusatzinformationen

Mehr über American Chemical Society Publications
Ihr Bowser ist nicht aktuell. Microsoft Internet Explorer 6.0 unterstützt einige Funktionen auf Chemie.DE nicht.